Wanna discuss the problem as we are all facing it.
I've tried both Sylgard 184 and FEP teflon.
Of course Sylgard dies really fast, that's a pain, and really hard to work with, but it has almost perfect non-sticking capabilities.
Recently I tried also FEP teflon adhesive from CS Hyde.
At first I was surprised that it will last much longer, but later I noticed that it has a very bad non-sticking capabilities comparing to PDMS.
So even small prints now require TILTING:( That's not cool at all.
I'm using MakerJuice resin.
Any ideas, advice please?
I'm pretty stuck with separation layer problem...
Teflon should be a great option, but what am I doing wrong?
Thanks in advance,Statistics: Posted by zerospace — Wed Feb 19, 2014 10:17 pm
]]>